Nichrome, Manganin and Constantan: Alloys With Weak Temperature Dependence
On this page· 13 sections
Source & scope. Class 12 Physics, Chapter 3 Current Electricity, Section 3.8 Temperature Dependence of Resistivity (the alloys portion). Builds on: Temperature Dependence of Resistivity in Metals, which establishes that pure metals have a strongly positive, near-linear resistivity-temperature relati...
Source & scope. Class 12 Physics, Chapter 3 Current Electricity, Section 3.8 Temperature Dependence of Resistivity (the alloys portion). Builds on: Temperature Dependence of Resistivity in Metals, which establishes that pure metals have a strongly positive, near-linear resistivity-temperature relation. Next: Temperature Dependence of Resistivity in Semiconductors, covering the opposite-direction case.
Nichrome — an alloy of nickel, iron and chromium — exhibits a very weak dependence of resistivity on temperature, a property shared by manganin and constantan. Because the resistance of these alloys changes very little as temperature changes, they are widely used in wire-bound standard resistors, where NCERT's Fig. 3.9 plots nichrome's resistivity against absolute temperature to show just how flat that curve is compared with a pure metal.
At a glance
- Nichrome (nickel + iron + chromium alloy), manganin, and constantan all show a very weak resistivity-temperature dependence (Fig. 3.9, nichrome).
- This near-constant resistance with temperature is why these alloys are used in wire-bound standard resistors.
- Contrast: pure metals (copper, platinum) show resistance changing substantially and near-linearly with temperature — unsuitable where a stable reference resistance matters.
- Nichrome's high resistivity and physical robustness additionally make it the standard choice for heating elements (e.g., NCERT's toaster example).
- The alloying itself is what suppresses the temperature sensitivity seen in the corresponding pure metals.
Learning objectives
- Name the three alloys NCERT identifies as having weak resistivity-temperature dependence, and nichrome's composition.
- Explain why a near-temperature-independent resistance is desirable in a standard resistor.
- Contrast this alloy behaviour with the strong, near-linear temperature dependence of pure metals.
- Connect nichrome's two distinct NCERT-cited uses: standard resistors (weak T-dependence) and heating elements (high resistivity, robustness).
Prerequisite knowledge
The reader should already know the ρT = ρ0[1 + α(T − T0)] relation and that α is positive and significant for ordinary metals (covered in the sibling article on temperature dependence of resistivity in metals), since this article's point is that these particular alloys have an unusually small α by comparison.
Core explanation
Three named alloys with weak temperature dependence
NCERT singles out Nichrome — explicitly described as an alloy of nickel, iron and chromium — as exhibiting a very weak dependence of resistivity on temperature, illustrated in Fig. 3.9 as a plot of nichrome's resistivity rT against absolute temperature T. NCERT then states that manganin and constantan have similar properties: both are alloys whose resistivity likewise barely changes as temperature changes, placing all three in the same special category, distinct from ordinary pure metals like copper.
Why this matters: standard resistors
Because the resistance values of nichrome, manganin and constantan change very little with temperature, these materials are widely used in wire-bound standard resistors. A standard resistor is meant to provide a fixed, reliable, known resistance value for calibration and measurement; if its resistance drifted noticeably every time the ambient temperature or the current through it changed (as happens with a pure metal resistor), it would be useless as a stable reference. The weak temperature dependence of these alloys is exactly the property that makes them fit for this role.
Contrast with pure metals
This is the direct opposite of the behaviour of pure metals such as copper and platinum, whose resistivity changes substantially and nearly linearly with temperature over a limited range, as described by ρT = ρ0[1 + α(T − T0)] with a clearly positive α (covered in the sibling article). That strong, predictable temperature sensitivity is precisely why pure metals are not chosen where a stable reference resistance is needed — the very same property that makes platinum useful as a resistance thermometer (because its resistance tracks temperature reliably) makes it unsuitable as a standard resistor (because its resistance would not stay fixed). Alloys like nichrome, manganin and constantan solve this by suppressing that temperature sensitivity almost entirely.
A second, independent use of nichrome
Nichrome's resistivity profile also serves a second, separate purpose: its naturally high resistivity combined with physical robustness at high temperatures makes it the standard material for heating elements, such as the toaster element analysed in NCERT's Example 3.3 (reused in the sibling article on metal temperature dependence), which reaches a steady operating temperature of 847 °C without damage. This heating-element application depends on nichrome's high absolute resistivity value (so it dissipates significant heat for a practical current), which is a different property from — though compatible with — its weak temperature dependence, which is what makes it (and manganin, constantan) suitable for standard resistors.
Key terms
- Nichrome — an alloy of nickel, iron and chromium with weak resistivity-temperature dependence and high resistivity; used in standard resistors and heating elements.
- Manganin — an alloy with similarly weak resistivity-temperature dependence, used in standard resistors.
- Constantan — an alloy with similarly weak resistivity-temperature dependence, used in standard resistors.
- Standard resistor — a resistor built to provide a fixed, reliable resistance value for calibration/measurement, which requires minimal resistance drift with temperature.
- Temperature coefficient of resistivity (α) — near zero in magnitude for these alloys, versus clearly positive for pure metals.
Diagram / figure guidance
Draw two resistivity-vs-temperature curves on the same axes (mirroring the contrast between Fig. 3.8 and Fig. 3.9): one steep, clearly rising line labelled "pure metal (e.g. copper)", and one nearly flat, almost horizontal line labelled "nichrome / manganin / constantan". Annotate the flat line "near-constant resistance — ideal for standard resistors" and the steep line "large resistance change with T — unsuitable as a stable reference".
Worked example
A standard resistor is to be built to maintain a resistance close to 100.0 Ω across a laboratory temperature range of 20 °C to 35 °C, with a tolerance of no more than 0.05 Ω of drift. A manganin wire with temperature coefficient of resistance 3 × 10⁻⁵ °C⁻¹ and a copper wire with temperature coefficient of resistance 4.0 × 10⁻³ °C⁻¹ are both available, each cut to give 100.0 Ω at 20 °C. Which should be used, and by how much would each drift over this range?
For the manganin wire: ΔR = R0 × α × ΔT = 100.0 × 3×10⁻⁵ × 15 = 0.045 Ω — within the 0.05 Ω tolerance.
For the copper wire: ΔR = R0 × α × ΔT = 100.0 × 4.0×10⁻³ × 15 = 6.0 Ω — far outside the tolerance, nearly 6% drift.
The manganin wire should be used: its very weak temperature coefficient keeps the drift (0.045 Ω) within tolerance, while copper's much larger, near-linear temperature coefficient (as for any ordinary pure metal) produces a drift more than a hundred times larger, making it unusable as a stable standard resistor over this temperature range.
Common misconceptions
- "Nichrome is used in standard resistors and heating elements for the same reason." These are two distinct properties: weak temperature dependence (stability) justifies its use in standard resistors, while high resistivity and physical robustness justify its use in heating elements — NCERT presents them as separate facts.
- "Manganin and constantan are the same material as nichrome." They are three distinct named alloys; NCERT groups them together only because they share the property of weak resistivity-temperature dependence, not because they are chemically identical.
- "A material with weak temperature dependence must also have low resistivity." Temperature sensitivity (how much ρ changes with T) and the absolute value of ρ are independent properties — nichrome, for instance, has a weak temperature dependence yet a comparatively high resistivity, useful for heating elements.
- "Pure metals are never useful once we have these alloys." Pure metals like platinum are still essential precisely because their resistance does change predictably with temperature — that is the property exploited by a platinum resistance thermometer, covered in the sibling article.
Exam application (NEET & JEE)
Exam questions typically ask students to name the alloys with weak temperature dependence (nichrome, manganin, constantan) and their defining application (standard resistors), often as a direct-recall MCQ, or to explain why a stable reference resistor requires low temperature sensitivity rather than low resistivity. A frequent conceptual trap pairs this with nichrome's heating-element use, testing whether the student can correctly attribute each use to the right underlying property (temperature stability vs. high resistivity) rather than conflating the two.
Frequently asked questions
- Which alloys show weak dependence of resistivity on temperature? Nichrome (an alloy of nickel, iron and chromium), manganin, and constantan all exhibit a very weak dependence of resistivity on temperature.
- Why are nichrome, manganin and constantan used in standard resistors? Because their resistance values change very little with temperature, they provide a stable, reliable resistance value suitable for calibration and measurement instruments.
- Why aren't pure metals like copper used for standard resistors? Pure metals have resistivity that changes substantially and near-linearly with temperature, so a resistor made from them would drift noticeably as temperature changes, unlike these special alloys.
- Is nichrome used only for standard resistors? No — nichrome's high resistivity and robustness also make it the standard material for heating elements, such as toaster elements, a separate application from its use in standard resistors.
- What is nichrome made of? Nichrome is an alloy of nickel, iron and chromium.
Practice questions (original practice questions)
- Which of the following is an alloy explicitly named by NCERT as having a very weak dependence of resistivity on temperature?
- (a) Copper
- (b) Platinum
- (c) Nichrome
- (d) Silver
- Answer: (c) — Nichrome, along with manganin and constantan, shows very weak resistivity-temperature dependence.
- Nichrome is described in NCERT as an alloy of:
- (a) copper, zinc and tin
- (b) nickel, iron and chromium
- (c) iron, carbon and manganese
- (d) platinum, nickel and gold
- Answer: (b) — NCERT explicitly gives this composition.
- A wire-bound standard resistor is best constructed from a material whose resistivity:
- (a) changes strongly and linearly with temperature
- (b) changes very little with temperature
- (c) is exactly zero
- (d) decreases sharply with temperature like a semiconductor
- Answer: (b) — Stability of resistance with temperature is the key requirement for a standard resistor.
- Manganin and constantan are grouped with nichrome in NCERT's discussion because they:
- (a) are chemically identical to nichrome
- (b) are both semiconductors
- (c) also show weak resistivity-temperature dependence
- (d) are both used only as heating elements
- Answer: (c) — NCERT states manganin and constantan have "similar properties" to nichrome in this respect.
- A pure copper resistor and a manganin resistor are both built to 50.0 Ω at 20 °C. Heated to 40 °C, which resistor shows the larger resistance change, and why?
- (a) Manganin, because its resistivity is higher
- (b) Copper, because its temperature coefficient of resistivity is far larger
- (c) Both change identically
- (d) Neither changes at all
- Answer: (b) — Copper's much larger α (as for ordinary pure metals) produces a far bigger resistance drift than manganin's near-zero temperature coefficient.
Quick revision
- Nichrome (Ni + Fe + Cr alloy), manganin, and constantan all show very weak resistivity-temperature dependence (Fig. 3.9).
- This stability is why they're used in wire-bound standard resistors.
- Pure metals (copper, platinum) show strong, near-linear resistivity-temperature dependence — unsuitable as stable references.
- Nichrome's separate property — high resistivity + robustness — makes it the standard heating-element material (e.g., the toaster example).
- Temperature sensitivity and absolute resistivity value are independent properties of a material.
Related articles
- Builds on: Temperature Dependence of Resistivity in Metals
- See also: Temperature Dependence of Resistivity in Semiconductors, Platinum Resistance Thermometer
- Next: Electrical Power and Joule Heating
- Related topics: Cells in Parallel, Cells in Series, Current Density and Conductivity, Drift Velocity of Electrons, EMF (Electromotive Force) of a Cell, Electric Current — Definition and SI Unit